A. Because the inner lining of the steel-plastic composite drum is polyethylene, it is not suitable to fill the product above 55 ~C or to heat the product above 55 ~C in use. If this happens, the steel drum is easily damaged.

B. The inner lining of the steel-plastic drum is polyethylene, so the storage temperature is below 40 C. At the same time, the drum should be stored under canopy to avoid exposure to sunlight. If this is the case, the polyethylene lining of the steel-plastic drum is easily broken.

C. The steel-plastic composite drum has leak holes at the bottom of the outer drum according to the requirements of commercial inspection and industry standards. If no leak holes are required, special instructions are required.

Professional products.
Passionately applied.

Quick Links

Product Category

Social Media
Contact Info
Contact person:Amber Mao
Tel:+86-0510-85996239
Fax:+86-0510-85995017
Mobile:+86-15061817591
QQ:546468115
E-mail:amber@wxsfgroup.com
Contact Form
Copyrights © 2022 Wuxi Sifang Group Co., Ltd. All rights reserved   Sitemap | Support by Leadong